Designation: Z
Synonyms: White galvanized.
Price: from 10 rub. . per dm2
Please fill out the contact form so that we can process your request.
Your application has been successfully sent. We will contact you shortly. Please wait for the manager's call!
Continue workDesignation: Z
Synonyms: White galvanized.
Price: from 10 rub. . per dm2
Designation: Z
Synonyms: White galvanized.
Price: from 10 rub. per dm2
Purpose: White galvanic zinc plating - one of the main anti-corrosion coatings on steel.
Designation: Z
Synonyms: Zinc yellow
Price: from 10 rub. per dm2
Designation: Zn
Synonyms: Yellow galvanized.
Price: from 10 rub. per dm2
Purpose: Rainbow galvanizing is the main anti-corrosion coating for steel springs. Yellow chromate plating significantly increases the protective properties of the coating, second only to khaki passivation in terms of corrosion resistance. Springs with a tensile strength above 1380 MPa are usually not galvanized without heat treatment.
Designation: Zn.t
Synonyms: White galvanized.
Price: from 10 rub. . per dm2
Purpose: White galvanizing with heat treatment - anti-corrosion coating for high-strength steels.
Designation: Zn.black
Synonyms: Black galvanized
Price: from 10 rub. per dm2
Designation: Zn.olive
Synonyms: Green galvanized, olive zinc.
Price: from 10 rub. per dm2
Purpose: Olive galvanizing - a powerful anti-corrosion coating for steel with the most durable chromate passivation "khaki". This type of chromating provides a significant increase in the protective properties of zinc due to the greatest thickness of the outer film compared to analogues. Olive galvanizing is most often used on military parts operating in harsh conditions.
Designation: Zn
Synonyms: Zinc with phosphate.
Price: from 10 rub. per dm2
Designation: Zn-Ni
Synonyms: -
Price: from 10 rub. per dm2
Purpose: Zn-Ni - modified anti-corrosion coating for steel. Due to the 12-16% nickel content in the alloy, the coating becomes harder, more resistant to corrosion and high temperatures. The main application of the coating is in the automotive industry.
Just leave your request by filling out the form on the right and we will contact you as soon as possible. Thank you!
By submitting an application, you agree to processing of your personal data. Your data is protected.